Firing method: Oxidation and reduction possible Appropriate firing temperature: 1230-1300℃

[Shipping & Postage (International)]

有田焼の産地の呉須の製造メーカーでWeb上で直販しているのは深海商店だけです。

Q : 絵具がはじく原因は?

Firing temperature : Reduction: 1280℃ Oxidation: 1250℃

鉄赤結晶18(1.8L) 色:Elabo, Tenmoku, Crystal, Spot, Crazing, Yohen Firing method: Oxidation and reduction[Firing conditions for sample plates] Ceramic clay components For pottery: Umezaki red clay (SiO2 72. 11%, Al2O3 15. 98%, Fe2O3 2. 12%, TiO2 0. 67%, CaO 0. 12%, MgO 0. 36%, Na2O 0. 58%, K2O 2. 47%, Ig. Loss 5. 16%) Firing temperature : Reduction: 1280 Glazing : Baume concentration 50 (soak for about 3 seconds) [How to use] Soil type: porcelain, pottery Possible firing method: oxidation and reduction possible Appropriate firing temperature: 1230 1300

Exchange/Return Notes
  • We offer a 30-day return/exchange service after receiving.
  • Final sale items are not eligible for returns or exchanges.
  • To process your return/exchange, please contact us at [email protected]
  • Please click here for more details>>> Return & Exchange Policy

You may also like

recommand products